How to correctly distinguish and choose injection moulding materials PA6 and PA66?
How to correctly distinguish and choose injection moulding materials PA6 and PA66? With the development of modified nylon technology becoming more mature, the application range of PA6 and PA66 is gradually expanding. Many plastic mold factories or units that use nylon injection molding materials have no clear distinction between PA6 and PA66. In addition, the appearance of PA6 and PA66 are very similar. The obvious difference caused a lot of confusion. How to distinguish between PA6 and PA66 and how to choose? Identification tips for PA6 and PA66: Burned with burned wool and nails, PA6 is a light yellow flame, and PA66 is a blue flame. PA6 has good toughness, is cheaper than PA66, and has a low melting point (225 degrees). PA66 has good strength, wear resistance and high melting point (255 degrees). The physical difference between PA6 and PA66: The melting point of PA66 is 260 to 265°C, and the glass transition temperature (dry state) is 50°C. The density is 1.13~1.16 g/cm3. PA6 ...